The final surface treatment of the printed items yields an exceptional tactile quality. For enhanced refinement, it is recommended to utilize fine sandpaper in conjunction with water. This method effectively eliminates issues related to the removal of support structures during the 3D printing process. Weight: 0.75 kg.
SUGGESTED PRINT SETS (1) |
Suggested print sets | unit | value | test method |
extruder temp | C° | 220-240 | internal |
plate temp | C° | 90-110 | internal |
min. nozzle diameter | mm | 0,35 | internal |
fan | % | 0-20 | internal |
print speed | mm/1° | 60-70 | internal |
PROPERTY |
Physical | | | |
Water absorption | % | 0.2 | ISO 179 |
Mechanical at 23°C / 50% rh | | | |
Tensile modulus | MPa | 2500 | ISO 527 |
MFR | g/10 min | 4 | ISO 1133 |
Charpy impact (23°C) | ft·lb/in2 | 8 | ISO 179 |
Charpy impact (-30°C) | ft·lb/in2 | 3 | ISO 179 |
Thermal | | | |
Vicat softening temp. | °C | 102 | ISO 96 |